Engineering tool

Alloy selection tool — from voltage and power to wire length

Choose a grade, enter wire diameter, supply voltage, target power and working temperature. The tool uses resistivity, density and Ct tables published in our 2026 datasheets for 23 grades — FeCrAl, NiCr and CuNi — and carries the completed configuration into your enquiry.

1 · Your operating conditions

All values are theoretical estimates at 20 °C unless stated.

2 · Calculated configuration

Wire cross-section —mm²
Target resistance R20 —Ω
Current —A
Required wire length —m
Resistance per metre (20 °C) —Ω/m
Estimated mass —kg
Surface load —W/cm²
Ct at working temperature —×
R at working temperature —Ω
Power at temperature (constant U) —W

"Send this configuration for a quote" opens the enquiry form with the grade, diameter, voltage, power, temperature and calculated values already filled in — so our sales team receives a specification, not just "please quote".

How we calculate

Formulae, units and boundaries

These formulae are published here so that the result can be checked by hand and so that search and AI engines can quote the method accurately. ρ is the nominal 20 °C resistivity from the grade datasheet, in Ω·m.

QuantityFormulaNotes
Cross-sectionA = π d² / 4d in mm; convert to m² by ×10⁻⁶
Resistance from powerR20 = U² / PU in V, P in W, R in Ω at 20 °C
CurrentI = U / R20Ohm's law
LengthL = R20 · A / ρρ is the published resistivity in Ω·m at 20 °C
Resistance per metreΩ/m = ρ / Acompare with the datasheet wire table
Massm = A · L · densitydensity in kg/m³ (g/cm³ × 1000)
Surface areaS = π · d · Ld in cm, L in cm → cm²
Surface loadq = P / SW/cm²; theoretical, no heat-dissipation model
Temperature correctionR(T) = R20 × CtCt is listed on the product category page and downloadable datasheet
Power at temperatureP(T) = P20 / Ctonly valid at constant supply voltage
Boundaries. Ct tables cover 20–1300 °C where published; values outside that range, and grades without a published Ct table, are not estimated. Permissible surface load, heat-dissipation factors and winding corrections are not published in our supplied material and are deliberately absent. Real element design must account for furnace heat dissipation, winding geometry, temperature coefficient and mounting — confirm the final selection with our engineers.
Classic converters

Wire gauge & Ohm's law

Gauge → millimetres

—

AWG uses the ASTM B258 formula d = 0.127 × 92^((36−n)/39) mm. SWG inch values are taken from this site's original gauge calculator.

Ohm's law (enter any two)

—

FAQ

About the tool

Where do the resistivity values come from?

From the 2026 English datasheets supplied by Jiangsu Heyi. Where a datasheet publishes resistivity by wire-diameter band (for example Cr20Ni80: 1.09 / 1.13 / 1.14 µΩ·m), the tool selects the band that matches the diameter you enter.

Why is Ct shown as — for some grades?

Because no Ct temperature-factor table is published for that grade in the supplied datasheets. The tool does not estimate one; room-temperature results remain valid.

Does the tool tell me whether my surface load is safe?

No. It calculates W/cm², but the permissible surface load depends on furnace heat dissipation, winding geometry, atmosphere and mounting. Those limits are not published in the supplied material, so the tool does not invent a recommended range.

Can I use the result as a purchase specification?

Treat it as a theoretical starting point. Manufacturing tolerances, the temperature coefficient and installation conditions all affect the final element. Send the configuration to our engineers for confirmation.

Download the full datasheets →

Want an engineer to check the result?

Paste or send the configuration and we will verify the grade, diameter and surface load against your furnace conditions.